Food
Food name | Side stream | Component group | Component | Value | Unit | Description | Reference |
---|---|---|---|---|---|---|---|
Bamboo | Biochar from bamboo stems | Inorganics | Iron | 170 | mg/kg DM | Bambusa vulgaris. Biochar produced at ECN, pyrolysed slowly at 400°C for 60 min in an auger type (screw) pyrolyser (Pyromaat) | ECN Phyllis 2 |
Green waste | Biochar from green waste | Inorganics | Iron | 240 | mg/kg DM | Product from large scale gasification at 670°C | ECN Phyllis 2 |
Green waste | Biochar from greenhouse waste | Inorganics | Iron | 2155 | mg/kg DM | Pepper residues 600/60/0. Combustion temperature: 600°C, 60 minutes, 0% oxygen. Greenhouse waste biochar produced in the slow pyrolysis unit at ECN from greenhouse residues of pepper | ECN Phyllis 2 |
Green waste | Biochar from greenhouse waste | Inorganics | Iron | 660 | mg/kg DM | Pepper residues 600/60/1. Combustion temperature: 600°C, 60 minutes, 1% oxygen. Greenhouse waste biochar produced in the slow pyrolysis unit at ECN from greenhouse residues of pepper | ECN Phyllis 2 |
Green waste | Biochar from greenhouse waste | Inorganics | Iron | 4700 | mg/kg DM | Pepper residues under gasification. Combustion temperature: 670°C, gasification biochar from greenhouse residues of pepper | ECN Phyllis 2 |
Green waste | Biochar from greenhouse waste | Inorganics | Iron | 660 | mg/kg DM | Pepper residues under gasification. Combustion temperature: gasification at 750°C | ECN Phyllis 2 |
Straw | Straw | Inorganics | Iron | 100 | mg/kg DM | ECN Phyllis 2 | |
Straw | Straw pellets char | Inorganics | Iron | 6439.9 | mg/kg DM | Chinese straw pellets 350 deg C | ECN Phyllis 2 |
Straw | Straw pellets char | Inorganics | Iron | 8574.9 | mg/kg DM | Chinese straw pellets 550 deg C | ECN Phyllis 2 |
Cacao/cocoa | Cacao shells | Inorganics | Iron | 300 | mg/kg DM | ECN Phyllis 2 |