Food
Food name | Side stream | Component group | Component | Value | Unit | Description | Reference |
---|---|---|---|---|---|---|---|
Coconut | Coconut fibre dust | Proximates | Ash | 2.9 | % | Coir. Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Proximates | Ash | 3.72 | % | Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Inorganics | Carbon | 47.17 | % | Coir. Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Inorganics | Carbon | 50.29 | % | Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Inorganics | Carbon, fixed | 26.8 | % | Coir. Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Inorganics | Carbon, fixed | 29.7 | % | Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Inorganics | Chlorine | 2800 | mg/kg | Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Waste compounds | Fluid temperature | 1170 | °C | Coir. Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Waste compounds | Heating value, high | 18.2 | MJ/kg | Coir. Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |
Coconut | Coconut fibre dust | Waste compounds | Heating value, high | 20.05 | MJ/kg | Devolatilisation occurs between 330 and 600°C, maximum rate at 350°C | ECN Phyllis 2 |